Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 621 - 827 MPa @Thickness <=25.4 mm |
90000 - 120000 psi @Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Tensile Strength | 655 - 827 MPa | 95000 - 120000 psi | Escomatic Coils |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Tensile Strength | 655 - 827 MPa @Thickness <=25.4 mm |
95000 - 120000 psi @Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 303 HD Stainless Steel Bar Description: 303 UGIMA HD™ is a low sulfur version of Ugitech’s improved machining 303 grade. It is designed to provide better metallurgical performance with respect to weldability, corros.. |
|||
Tensile Strength | 655 - 827 MPa | 95000 - 120000 psi | Escomatic Coils |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Tensile Strength | 655 - 827 MPa @Thickness <=25.4 mm |
95000 - 120000 psi @Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 303 Stainless Steel Bar Description: 303 UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 303, except with respect to machinability. 303 UGIMA® repre.. |
|||
Tensile Strength | 331 - 827 MPa | 48000 - 120000 psi | |
Chicago Extruded Metals BioBrass® UNS C27000 Copper-Zinc Alloy Finished product available as wire, rod, or tube.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extrude.. |