Polymer Property : Tensile Strength = 621 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 414 - 621 MPa
60000 - 90000 psi
Eagle Brass 200/201 Nickel Alloy, 1/2 Hardened
Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick..
Tensile Strength 483 - 621 MPa
70000 - 90000 psi
Eagle Brass 200/201 Nickel Alloy, 3/4 Hardened
Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick..
Tensile Strength 538 - 621 MPa
78000 - 90000 psi
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
Tensile Strength 552 - 621 MPa
80000 - 90000 psi
Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy
Finished product available as bar, wire, or rod.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Meta..
Tensile Strength 276 - 621 MPa
40000 - 90000 psi
Chicago Extruded Metals BioBrass® UNS C22000 Copper-Zinc Alloy
Finished product available as bar or wire.Chicago Extruded Metal temper codes: H01, H02, H04This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Metal..
Tensile Strength 483 - 621 MPa

@Thickness <=25.4 mm
70000 - 90000 psi

@Thickness <=1.00 in
Cold Drawn Bars
Schmolz + Bickenbach IMRE™ Stainless Steel Bar
Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand..