Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 33.1 - 46.9 MPa | 4800 - 6800 psi | |
Bulk Molding Compounds BMC A30 General Purpose Molding Compound BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol.. |
|||
Tensile Strength | 33.1 - 46.9 MPa | 4800 - 6800 psi | |
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the .. |