Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.0 - 30.0 MPa | 2900 - 4350 psi | Injection; ISO 527 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Tensile Strength | 25.0 - 30.0 MPa | 3630 - 4350 psi | DIN 53288 |
Permabond TA439 Toughened Acrylic Adhesive Permabond® TA439 is a two component structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some plastics. The typical fixture time of is 10-30 seconds. The fast f.. |
|||
Tensile Strength | 20.0 - 30.0 MPa @Temperature 25.0 °C |
2900 - 4350 psi @Temperature 77.0 °F |
stainless steel after 24 hours |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Tensile Strength | 20.0 - 30.0 MPa @Temperature 25.0 °C |
2900 - 4350 psi @Temperature 77.0 °F |
stainless steel after 24 hours |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Tensile Strength | 25.0 - 30.0 MPa | 3630 - 4350 psi | DIN 53455 |
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 20.0 - 30.0 MPa | 2900 - 4350 psi | ISO 527 |
Isoflon Virgin PTFE Polytetrafluoroethylene Properties/Improved compression and wear resistanceExcellent chemical stabilityBetter thermal conductivityExcellent resistance to continuous service temperatures up to 260°C, and, for limited per.. |
|||
Tensile Strength | 20.0 - 30.0 MPa | 2900 - 4350 psi | DIN 53455 |
Isoflon PTFE Polytetrafluoroethylene Fluoropolymer material specifications.Information provided by Isoflon. |