Mechanical Properties Metric English Comments
Tensile Strength 20.0 - 25.0 MPa
2900 - 3630 psi
DIN 53455
Isoflon FEP Fluorinated Ethylene Propylene
Fluoropolymer material specifications.Information provided by Isoflon.
Tensile Strength 20.0 - 25.0 MPa
2900 - 3630 psi
ASTM D4894
Isoflon PTFE + 40% Bronze Polytetrafluoroethylene with 40% Bronze
Properties:Excellent wear and compression resistance (low cold creep)Good thermal conductivityImproved coefficient of friction when combined with Mos² or graphiteApplications: Dynamic seals for ..
Tensile Strength 13.5 - 25.0 MPa
1960 - 3630 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is..
Tensile Strength 12.0 - 25.0 MPa
1740 - 3630 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..
Tensile Strength 13.5 - 25.0 MPa
1960 - 3630 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 018 85% Virgin PTFE, 15% Graphite
Applications & Industries: General: Graphite filler improves the sliding properties & thermal conductivity of PTFE and has one of the lowest coefficient of frictions. It has low wear in water and is..
Tensile Strength 12.0 - 25.0 MPa
1740 - 3630 psi
Moulding Direction; BS2782:Pt3
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..