Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 18.0 - 23.0 MPa | 2610 - 3340 psi | ASTM D4894 |
Isoflon PTFE + 15% Ceramic Polytetrafluoroethylene with 15% Ceramic Properties:Improved compression resistanceGood dielectric characteristicsGood thermal insulationMachining can be trickyApplications: Electrical applicationsInformation provided by Isoflon. |
|||
Tensile Strength | 18.0 - 23.0 MPa | 2610 - 3340 psi | ASTM D4894 |
Isoflon PTFE + 15% Graphite Polytetrafluoroethylene with 15% Graphite Properties:Good thermal conductivityLow coefficient of frictionLow permeabilityApplications: Non-lubricated dynamic seals.Information provided by Isoflon. |
|||
Tensile Strength | 17.0 - 23.0 MPa | 2470 - 3340 psi | molded; ASTM D4745 |
Guarniflon PTFE G420 Polytetrafluoroethylene 50% Steel PTFE G Special Compound with steelInformation provided by Guarniflon® |
|||
Tensile Strength | 17.0 - 23.0 MPa | 2470 - 3340 psi | molded; ASTM D4894, ASTM D4745 |
Guarniflon PTFE G458 Polytetrafluoroethylene 60% Bronze, 2% Carbon PTFE G Standard Compound with bronzeProperties: Enhanced compressive strength. Good wear resistance and high thermal conductivity.Application: Unlubricated bearings for high speed excluding hard .. |