Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.00 - 13.0 MPa | 1160 - 1890 psi | molded; ASTM D4745 |
Guarniflon PTFE G455 Polytetrafluoroethylene 35% Carbographite PTFE G Special Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high w.. |