Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 9.00 MPa | >= 1310 psi | Type IV, 500mm/min; ISO 37 |
S&E Specialty Polymers XP44-10MG PVC Description: PVC weatherable, integral colored, filledApplication: Body side end cap molding compound which meets the GMP.PVC.002 & GMP.PVC.014.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 9.00 MPa | 1310 psi | ISO 37 |
Termopol Termoton® V6GA3075A TPV Compound Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Addisilâ„¢ 482 E Healthcare Extrusion Grade Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6045 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LIM 6061 Liquid Silicone Rubber - Fast Cure / High Tear This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2040 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2070 Liquid Silicone Rubber - General Purpose This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2661 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2671 Liquid Silicone Rubber - Non Post Cure / Low Compression Set This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 2752 Liquid Silicone Rubber - Self-Bonding This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3285/50 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3286/60 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4040 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4070 Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 4630 FC Liquid Silicone Rubber - Healthcare LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding .. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Silplusâ„¢ 30 HS High Strength Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Silplusâ„¢ 40 MP Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | Flatwise |
Henkel Hysol EA 9696 Film Adhesive Second generation, moisture-resistant, toughened 250°F / 121°C service, modified epoxy film. Qualified to BMS 5-101 and BMS 5-129. Data from .060 psf, 300 g / m2.Applications: Composite Bondin.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Momentive Performance Materials Siloprenâ„¢ LSR 3485/35 Liquid Silicone Rubber - Self-Lubricating / Standard This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva.. |
|||
Tensile Strength | 9.00 MPa | 1310 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-40AB Elastomer KE-2090-40 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Tensile Strength | 9.00 MPa @Strain 20.0 % |
1310 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan 1198 A TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | >= 9.00 MPa | >= 1310 psi | |
AlphaGary Megolon™ FB119 Low Smoke Halogen Free Filling and bedding grade to meet the requirements of BS6724. Application examples include Radio Frequency / Data Optical / Special Fire Survival |
|||
Tensile Strength | >= 9.00 MPa | >= 1310 psi | Type IV, 500mm/min; ISO 37 |
S&E Specialty Polymers XP11-289A1MG PVC Description: PVC weatherable, integral colored, filledApplications: Body side end cap molding compound which meets GMW16084 Type 4, Grade I, Class B, GMP.PVC.002.Information provided by S&E Specialt.. |