Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.62 MPa | 1250 psi | ASTM D638 |
S&E Specialty Polymers G-94-142A PVC Application: Flexible Clear PVC based compound for extrusion and molding application.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 8.62 MPa | 1250 psi | ASTM D412 |
S&E Specialty Polymers TufGuard E™ XP-115DD-Zeta PE, Flame Retardant Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 8.62 MPa | 1250 psi | ASTM D412 |
S&E Specialty Polymers TufGuard E™ XP-115D-Zeta PE, Flame Retardant Application: Chlorinated PE TPO based compound suitable for Wire and Cable applications.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 8.62 MPa | 1250 psi | ASTM D412 |
Northstar Polymers MPP-D65A Polyether Base Polyurethane Resin MPP-D65A is a polyether base 2-component polyurethane resin casting system for molding and potting applications. It has a long pot-life and gradual curing pattern to provide easier handling for mol.. |
|||
Tensile Strength | 8.62 MPa @Strain 100 % |
1250 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B8502 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne |
|||
Tensile Strength | 8.62 MPa | 1250 psi | |
Teknor Apex Elexar® EL 3954-90 Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop.. |
|||
Tensile Strength | 8.62 MPa | 1250 psi | Compound Property; ASTM D412 |
Arlon 10842S018 0.018" (0.457 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Tensile Strength | 8.62 MPa | 1250 psi | Silicone Property; Arlon SQA-TMS-008 |
Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate Mar Resistant Press Pad - Product is sold with two finishes options: 55833R062AC - "C-finish" and 55833R062DST - "Smooth with Talc"Design/Construction:Interleave: 3 mil PESide 1: Cured Silicone Ru.. |
|||
Tensile Strength | 8.62 MPa | 1250 psi | Silicone Property; ASTM D412 |
Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used .. |