Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 72.0 MPa | 10400 psi | ISO 527-1 |
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Tensile Strength | 72.0 MPa | 10400 psi | DIN 53455 |
Isoflon PMMA Polymethyl-methacrylate Products with good mechanical performances under friction and good dimensional stability, notably in moist environmentsVery rigid, hardHigh machining precisionInformation provided by Isoflon. |
|||
Tensile Strength | 72.0 MPa | 10400 psi | ISO 527 |
Lucite International Diakon® Frost 952 70 Acrylic Polymer Information provided by Lucite International |
|||
Tensile Strength | 72.0 MPa | 10400 psi | ISO 527 |
Lucite International Diakon® Frost 952 80 Acrylic Polymer Information provided by Lucite International |
|||
Tensile Strength | 72.0 MPa | 10400 psi | ASTM D638 |
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Tensile Strength | 72.0 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
5mm/min (0.2in/min); ASTM D638 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Tensile Strength | 72.0 MPa @Temperature 23.0 °C |
10400 psi @Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers VESPEL TP-8929 Polyimide DuPont Vespel TP-8929 parts are specified for mechanical and thermal performance. TP-8929 parts offer low friction, dimensional stability, low outgassing, radiation resistance, and creep resistance... |