Mechanical Properties Metric English Comments
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite Optix® CA - 75 HID General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite Optix® CA - 75 LL General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite Optix® CA - 75 OG General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite Optix® CA - 75 UVA General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite West Optix® CA - 75 HID General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite West Optix® CA - 75 UVA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite West Optix® CP - 75 HID General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite West Optix® CA - 75 LL General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite West Optix® CP - 75 UVA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 71.0 MPa
10300 psi
Henkel Hysol Benzoxazine 99110 Infusion Resin
One-part Infusion resin for RTM & VARTM processing. Low viscosity, high hot-wet properties and very good resistance against flame, smoke and toxicity.
Tensile Strength 71.0 MPa
10300 psi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified
Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance..
Tensile Strength 71.0 MPa
10300 psi
ASTM D412
Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, ..
Tensile Strength 71.0 MPa
10300 psi
Machine; ASTM D882
Arlon CuClad 233 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate
CuClad 233 uses a medium fiberglass/PTFE ratio to balance lower dielectric constant and improved dissipation factor without sacrificing mechanical properties.Cross Plied Woven Fiberglass, alternatin..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite Optix® CP - 75 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite Optix® CP - 75 UVA General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite West Optix® CA - 75 OG General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Tensile Strength 71.0 MPa
10300 psi
ASTM D-638
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..