Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 70.0 MPa | 10200 psi | ASTM D638 |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Injection; ISO 527 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | DIN 53455 |
Isoflon PC Polycarbonate Good impact resistance among transparent materialsInformation provided by Isoflon. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | DIN 53455 |
Isoflon PSU Polysulfone Electrical insulating productsRigidHigh chemical, fire and temperature resistanceInformation provided by Isoflon. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | ISO 527 |
Lucite International Diakon® CLG340 Acrylic Polymer Information provided by Lucite International |
|||
Tensile Strength | 70.0 MPa | 10200 psi | ISO 527 |
Lucite International Diakon® ST15G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PA/PP 7500 GF 7/1 Polyamide/Polypropylene Medium viscosity special compound with increased rigidity and low moisture absorption.Application: For molding parts with high mechanical requirements at low moisture absorption.Information provide.. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe PF CP 204 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in electrical and electronic applications. Good stability of electrical properties under high humidity. Also available in cold or hot-punching versions.Information provided by Hippe. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe PF CP 206 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions.Information provided by Hippe. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe PF CP 308 Cellulose Paper Reinforced Phenolic Resin - Sheet Used in mechanical and electrical applications. Good electrical properties under normal humidity. Also available in hot-punching versions. Flame retardant.Information provided by Hippe. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe UP GM 201 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature.Information provided by Hippe. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe UP GM 202 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant.Information provid.. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Tensile Strength | 70.0 MPa @Strain 10.0 %, Temperature 0.000 °C |
10200 psi @Strain 10.0 %, Temperature 32.0 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | 50 mm/min; ISO 37 |
BASF Elastollan R 2002 25% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | >= 70.0 MPa | >= 10200 psi | IEC 1212-2 5.7 |
Hippe UP GM 203 Woven Glass Mat Reinforced Polyester (unsaturated) Resin - Sheet Used in mechanical and electrical applications. Good stability of electrical properties under high humidity. Good mechanical properties at moderate temperature. Flame retardant. With improved re.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Compression; ISO 527 |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Tensile Strength | 70.0 - 100 MPa | 10200 - 14500 psi | Compression; ISO 527 |
Raschig Group RALUPOL® 8605 UP Polyester Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Compression; ISO 527 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | DIN 53455 |
Isoflon PA 6 Polyamide 6 General use for mechanical partsGood heat resistanceEasy to useHigh moisture regainInformation provided by Isoflon. |
|||
Tensile Strength | 70.0 MPa | 10200 psi | ISO R527, 5 mm/min |
Lucite International SW Sanitary Ware Acrylic Sheet Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International |