Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.93 MPa @Strain 100 % |
1150 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3853 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A1030-R008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 2 inches width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A1030-X008-12 0.030" (0.762 mm) Fully Cured Fusible Silicone Rubber - Extruded Fusible Tape
(disco 1 inch width and 36 inches long. Design/Construction: Interleave: Polyester Film Extruded Fusible Tape (Rectangular Cross Section): Fully Cured Fusible Silicone RubberThis data represents typical v.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A3020-R004-12 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
  1 inch width and 36 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Prod.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
&nb 2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Th.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Transverse Direction; Injection molded sample tested at 10 in/min with Die D; ASTM D412 |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | |
Teknor Apex Tekbond® TB 1372A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | |
Teknor Apex Tekbond® TB 1415A Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | >= 7.93 MPa | >= 1150 psi | Compound Property |
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. .. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 31940C025 0.025" (0.635 mm) Uncured Silicone Rubber on HDPE Carrier Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberCarrier: HDPEThis data represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 55946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Side 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production materi.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-10R##-P2 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Certified to meet all requirements of US Military Specification A-A5.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; Arlon SQA-TMS-009 |
Arlon 920-10Hxx-P0 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, yellow, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.D.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 920-10R##-P2 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 930-10Bxx-P0 0.030" (0.762 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 30 mil thick, Black, Rectangular cross-section, Self-fu.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Tape Property; ASTM D412 |
Arlon LW201R##-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW201R##-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW201R##-P2 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) Description: Level Wrap®: 1 inch wide, 20 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW401B##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW50125Rxx-P0 0.050" (1.27 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1.25 inch wide, 50 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Design/Construction: Interleave: Polyethylene Rubber: Cured Self-Fusing Silicone Rubber Cross-Se.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 51946C030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat Appearance: Brown silicone rubber and gum on fiberglass.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 912-10X##-P0 0.012" (0.305 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 12 mil thick, Gray, Rectangular cross-section, Self-fus.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-10R##-P1 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-15X##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1.5” Wide Rectangular 1.5 inch wide, 15 mil thick, Gray, Rectangular cross-section, Self.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-20R##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 2” Wide Rectangular 2 inch wide, 15 mil thick, Red, Rectangular cross-section, Self-fusi.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon LW401B##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported) Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length.. |
|||
Tensile Strength | 7.93 MPa | 1150 psi | Silicone Property; ASTM D412 |
Arlon 915-10R##-P0 0.015" (0.381 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular Arlon Rectangular Tape: Rectangular tape is of uniform thickness and.. |