Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.80 MPa | 1130 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-60A/B Elastomer KE-1950-60 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Tensile Strength | 7.80 MPa | 1130 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-70A/B Elastomer KE-1950-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |