Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 7.24 MPa @Strain 100 % |
1050 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible C8500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 7.24 MPa @Strain 100 % |
1050 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3772 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 7.24 MPa | 1050 psi | ASTM D412 |
S&E Specialty Polymers TufTech™ GA-7565FR PVC Compound Application: A 75°C Matte finish jacketing compound.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 7.24 MPa | 1050 psi | Typical |
Garlock 502 Silicone Sheet Rubber Style #502 will be used in sealing applications that require resistance to extreme temperatures, high ozone concentrations, and high ultraviolet content.Information provided by Garlock Rubber Techno.. |
|||
Tensile Strength | 7.24 MPa @Strain 100 % |
1050 psi @Strain 100 % |
ASTM D638 |
Teknor Apex APEX® 3310-80NT Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Food Service Applications; Medical/Healthcare Applications; Tubing Processing Forms: Extrusion Forms: PelletsInformation Provided by Tek.. |
|||
Tensile Strength | 7.24 - 8.62 MPa | 1050 - 1250 psi | Compound Property |
Arlon 51943C014 0.014" (0.356 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |