Mechanical Properties Metric English Comments
Tensile Strength 62.0 MPa
8990 psi
at Break (NYP); ISO 527-1/-2
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data)
Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l..
Tensile Strength 62.0 MPa
8990 psi
ASTM D638
Kolon KOCETAL® K300EW Standard Grade Acetal Resin
General injection molding grade, toughness is slightly improved. Applications: General injection molding products.Information provided by API-Kolon.
Tensile Strength 62.0 MPa
8990 psi
ASTM D638
Kolon KOCETAL® LF701 Wear Modified Acetal Resin
Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon.
Tensile Strength 62.0 MPa
8990 psi
ASTM D638
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin
Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon.
Tensile Strength 62.0 - 69.0 MPa
8990 - 10000 psi
specimen type 1, 5 mm/mn; ASTM D638
Lucite International XL Sanitary Ware Acrylic Sheet
Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an..
Tensile Strength 62.0 MPa

@Strain 14.0 %,
Temperature 40.0 °C
8990 psi

@Strain 14.0 %,
Temperature 104 °F
50 mm/min; ISO 527-2
BASF Elastollan R 3000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 62.0 MPa

@Temperature 23.0 °C
8990 psi

@Temperature 73.4 °F
DAM; ASTM D638
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612  (Unverified Data**)
Zytel® FE3734 NC010 is an unreinforced, lubricated polyamide 612 resin suitable for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength 62.0 MPa
8990 psi
ISO 527-1
Sax Polymers SAXATEC 4115 Acrylonitrile Styrene Acrylate
SAXATEC 4115 is a medium viscosity, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX ..
Tensile Strength 62.0 MPa
8990 psi
ISO 527-1
Sax Polymers SAXATEC 4120 Acrylonitrile Styrene Acrylate
SAXATEC 4120 is a easy lowing, weatherable ASA injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Information provided by SAX Polym..