Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 6.55 MPa @Strain 100 % |
950 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2175 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2175 is a 75 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2175 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength | 6.55 MPa @Strain 100 % |
950 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3683 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 6.55 MPa @Strain 100 % |
950 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3785 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 31580R020 0.020" (0.508 mm) Uncured Silicone Rubber on HDPE Carrier
(discontinued **) Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: High Density PolyethyleneAppearance: Red silicone gum on polymer linerThis data represents typical values for the.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | |
Teknor Apex Tekbond® TB 1339B Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | ASTM D412 |
Teknor Apex Telcar® OBC 2419B Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 18596R026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 2; ASTM D412 |
Arlon 19586R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the production mat.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 32580R035 0.035" (0.889 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. .. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 51586R015E 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 51586R015H 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 51586R052 0.052" (1.32 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothInterleave: Polyethylene.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 1 Uncured Silicone Property; ASTM D412 |
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 2 Silicone Property; ASTM D412 |
Arlon 51588R015 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPETh.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 1, Silicone Property; ASTM D412 |
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 2, Layer 2, Silicone Property; ASTM D412 |
Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearanc.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 55581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum on.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 55586R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneAppearance: Red silicone gum and rubber on fiberglass clothTh.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 55589R032 0.034" (0.864 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 56596R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 99580R010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Interleave: FEP FilmSide 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassFlexible heater substrateAppearance: Red, High viscosity gum on release linersThis data repres.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 51581B015 0.015" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 51581R027 0.027" (0.686 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; Arlon SQA-TMS-008 |
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Side 2, Silicone Property; ASTM D412 |
Arlon 55586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEAppearance: Red silicone gum and rubber on fiberglass clothThis data .. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Layer 1, Silicone Property; ASTM D412 |
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Tensile Strength | >= 6.55 MPa | >= 950 psi | Compound Property |
Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 32580R030 0.030" Uncured Silicone Rubber on PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" PETThis data represents typical values for the production material and should not be used as mate.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 44580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate)This data represents typical values for the producti.. |
|||
Tensile Strength | 6.55 MPa | 950 psi | Silicone Property; ASTM D412 |
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc.. |