Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 50.0 MPa | >= 7250 psi | ASTM D882 |
OCTAL DPET™/PE Laminate Sheet with Improved Barrier Properties Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ASTM D638 |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ASTM D638 |
Premix Premi-Glas® 2203-20 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Excellent stiffness to weight rat.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ASTM D638 |
Premix Premi-Glas® 2205-20 CRSX Polyester SMC Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ASTM D638 |
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Tensile Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | Injection; ISO 527 |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Tensile Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | Injection; ISO 527 |
Raschig Group DECAL® 1760 Phenolic Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an.. |
|||
Tensile Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | Injection; ISO 527 |
Raschig Group DECAL® 2061 Phenolic Wood flour reinforced phenolic molding compound. Good electrical properties, chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals and PCAs and .. |
|||
Tensile Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | Injection and Compression; ISO 527 |
Raschig Group DECAL® 5431 Phenolic Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/.. |
|||
Tensile Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | Compression; ISO 527 |
Raschig Group DECAL® 572R Phenolic Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati.. |
|||
Tensile Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | Compression; ISO 527 |
Raschig Group DECAL® 666/8 Phenolic Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod.. |
|||
Tensile Strength | 50.0 - 90.0 MPa | 7250 - 13100 psi | Injection; ISO 527 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Tensile Strength | 50.0 - 70.0 MPa | 7250 - 10200 psi | ISO 527 |
Raschig Group RALUPOL® 2200 UP Polyester Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ASTM D638 |
Kolon KOCETAL® EL302 Toughened Grade Acetal Resin Flexible grade. Applications: Flexible products. Information provided by API-Kolon. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 527 |
Lucite International Diakon® CRG812 Acrylic Polymer, Toughened Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 527 |
Lucite International Diakon® TD735 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Tensile Strength | >= 50.0 MPa | >= 7250 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hb DL Polyphenylene Sulfide Resin Extrusion, low chlorineInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Tensile Strength | >= 50.0 MPa | >= 7250 psi | GB/T 1040.2-2006 |
Sichuan Deyang Haton® hb Polyphenylene Sulfide Resin Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 527-1 |
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene Saxalac 310A is a medium viscosity, impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 37 |
BASF Elastollan 1198 A TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 37 |
BASF Elastollan 690 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 37 |
BASF Elastollan B 80 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 37 |
BASF Elastollan C 59 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 37 |
BASF Elastollan C 75 A HPM TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 50.0 MPa @Strain 8.00 %, Temperature 60.0 °C |
7250 psi @Strain 8.00 %, Temperature 140 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 3000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 37 |
BASF Elastollan C 75 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 50.0 MPa @Strain 10.0 %, Temperature 40.0 °C |
7250 psi @Strain 10.0 %, Temperature 104 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | >= 50.0 MPa | >= 7250 psi | ISO 37 |
Austin Novel Materials Texalan® 664D Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Strength | 50.0 MPa | 7250 psi | ISO 37 |
BASF Elastollan 695 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |