Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.55 MPa | 805 psi | Silicone Property; ASTM D412 |
Arlon CP-499CA Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |