Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 5.52 MPa | >= 800 psi | Silicone Property; ASTM D412 |
Arlon R35551X014 0.014" (0.356 mm) Uncured Rubber with Coated Nextel Substrate
(discontinued **) Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberSubstrate: Coated Nextel This data Represents typical values for the production material. The data should not be used to write, or in .. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Compound Property; ASTM D412 |
Arlon R36772R008 0.008" (0.203 mm) Fully Cured, Unsupported, Silicone Rubber with Fiberglass Substrate
( Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material .. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Typical |
Garlock 50 Natural/SBR Sheet Rubber Blend of natural and SBR rubber, specially compounded to be quick-sealing, non-hardening and heat resistant.Red, cloth finish, drum curedInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 30090R022 0.022" (0.559 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The d.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 32140R062 0.062" (1.57 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 55146R040 0.040"(1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 55578XC028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 55579R043 0.043" (1.09 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production materi.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 55580R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 56106R026 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon CP-301C Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon CP-475R Bulk Compound Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arl.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Silicone Property |
Arlon R32390B020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassAll ingredients of product are listed in 21 CFR 177.26000This data represe.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon R37642R062 0.062" (1.57 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Interleave: PolyethyleneSide 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, mater.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 44566R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 49090R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data should not be used to wr.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 49091R010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data s.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 51586B015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum and rubber on fiberglass clothThis data Represents typical values for the production m.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 55102R024 0.024" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.In.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 55103R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materia.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 55276R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon R31651R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon R33089X028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon R34688XA030 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured/Cured LayersThis data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 44141R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Clear PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass Side 2: Uncured Silicone RubberInterleave 2: Blue PolyethyleneThis data represent.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 31140R020 0.020" (0.508 mm) Uncured Fluorosilicone Rubber on Release Carrier Design/Construction: Interleave: PolyethyleneProduct: Uncured Fluorosilicone Rubber Carrier: Release coated HDPE Product Use: Flexible heater insulationAppearance: Red silicone gum on polymer releas.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 44570R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 47573R007 0.0075" (0.190 mm) Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Cured Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifica.. |