Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638 |
Quadrant EPP TIVAR® Oil Filled UHMW-PE FDA/USDA Oil-Filled UHMW-PE (ASTM Product Data Sheet) |
|||
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638 |
Teknor Apex Chemlon® 275H Nylon 6, Copolymer, Impact Modified Notes: Very high impact and elongation, low flexural modulus material for tubing and wire jacketing applications requiring a soft, flexible product; FMVSS Flammability: Passes, FMVSS 302Processing M.. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638 |
Techmer ES Luriblend® ABS TX15 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638, ASTM D1708 |
ScanTube ETFE Tubing Information provided by ScanTube, Inc. |
|||
Tensile Strength | >= 44.8 MPa | >= 6500 psi | |
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable .. |
|||
Tensile Strength | >= 44.8 MPa | >= 6500 psi | |
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic.. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D412 |
Lubrizol ESTANE® 58309 Ether Based Thermoplastic Polyurethane Features: Good Physical Properties and Reduced Surface Tack.Uses: Flat Die/Cast Film and Blown Film Extrusion, Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInfo.. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638 |
Ecomass® 1700CO93 Copper Powder Filled Polyamide, Injection Molding High Specific Gravity, Copper Powder Filled Polyamide (PA), Rigid, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing applicationsInform.. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | IPC TM-650 2.4.18.3 |
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg 85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia.. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638 |
Americas Styrenics MC3650 High Heat Crystal Polystyrene Product CharacteristicsImproved cycle times in hard to fill partsExcellent clarity with slight blue tintFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsHousewaresConsumer.. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | IPC TM-650 2.4.18.3 |
Arlon 51N Lead-Free Compatible Epoxy Low-Flow 51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili.. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638 |
Aaron Industries AAROPRENE® AE PC/ABS 7000-2 PC/ABS Engineered Resin Melt flow index may be specified. |
|||
Tensile Strength | 44.8 MPa | 6500 psi | ASTM D638 |
Aaron Industries AAROPRENE® GFPP 2020 Glass Filled Polypropylene AAROPRENE® GFPP 2000 Series Glass Reinforced CompoundsMelt flow index may be specified. Color may be specified. |