Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 40.00 MPa | 5801 psi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® 11T80 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T80 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical pr.. |