Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 40.0 MPa | 5800 psi | ISO 527 |
Premix Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC Description: Premi-Glas® 1266 is a glass reinforced thermoset molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injection/Co.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D638 |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D638 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet) |
|||
Tensile Strength | 40.0 MPa @Temperature 22.8 °C |
5800 psi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP TIVAR® 1000 Virgin (Natural & Color except Black) UHMW-PE |
|||
Tensile Strength | 40.0 - 60.0 MPa | 5800 - 8700 psi | Compression; ISO 527 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Tensile Strength | 40.0 - 65.0 MPa | 5800 - 9430 psi | Compression; ISO 527 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Tensile Strength | 40.0 - 70.0 MPa | 5800 - 10200 psi | Injection; ISO 527 |
Raschig Group RALUPOL® 804 UP Polyester Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
GRECO ISOTHANE 2090A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
GRECO ISOTHANE 3065D Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength | 40.0 - 55.0 MPa | 5800 - 7980 psi | DIN 53455 |
Isoflon ECTFE Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
GRECO ISOTHANE 1160D Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
GRECO ISOTHANE 1170D Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 527-1 |
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene Saxalac 310T is an antistatic, high impact resistant ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% RH.Information provid.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 527-1 |
Sax Polymers SAXLAC 310U Acrylonitrile Butadiene Styrene Saxalac 310U is an antistatic, high impact resistant and light stabilized ABS injection molding grade, characterized by good processability and high stiffness.Mechanical property data tested at 50% .. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 527-1 |
Sax Polymers SAXLAC 835U Acrylonitrile Butadiene Styrene Saxalac 835U is an antistatic, easy flowing light stabilized ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical prop.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1198 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-8280H Super Hard Polyether-Based TPU Low mold shrinkage, good impact resistance, perfect transparency, good mold release, fatigue resistance, chemical & hydrolytic resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan 695 AU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan B 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan C 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 37 |
BASF Elastollan SP 883 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tensile Strength | >= 40.0 MPa | >= 5800 psi | ISO 37 |
Austin Novel Materials Texalan® 390A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Strength | >= 40.0 MPa | >= 5800 psi | ISO 37 |
Austin Novel Materials Texalan® 485A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Strength | 40.0 - 50.0 MPa | 5800 - 7250 psi | ISO 527 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ISO 37 |
BASF Elastollan 664 DU TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan B 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 40.0 MPa @Strain 300 % |
5800 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 74 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 40.0 MPa | 5800 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1564 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 40.0 - 70.0 MPa | 5800 - 10200 psi | Injection; ISO 527 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |