Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D638 |
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D638 |
Premix Premi-Glas® 2103-22 CRSX Polyester BMC Premi-Glas® 2103-22 CR-SX is a 22% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D638 |
Premix Premi-Glas® 2103-22 CR-SX-HT Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-22 CR-SX-HT is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL .. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D638 |
Premix Premi-Glas® 2103-25 CRSX Polyester BMC Premi-Glas® 2103-25 CR-SX is a 25% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | at Break (NYP); ISO 527-1/-2 |
Quadrant EPP Semitron® ESd 225 POM-C, static dissipative, extruded (ISO Data) Semitron ESd 225 is an acetal based static dissipative material ideal for material handling operations. It is also an excellent choice for fixturing used in the manufacturing of hard disk drives or .. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D412 |
GRECO ISOTHANE 1095AE Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D412 |
GRECO ISOTHANE 1195A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | Weld; ASTM D638 |
Kuraray Genestarâ„¢ GP2450NH-2 Nylon, 45% Glass Filled Standard V-0 Grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm.This grade meets UL94, V-0.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ISO 527 |
Lucite International Diakon® ST45G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ISO 527 |
Lucite International Diakon® TD642 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D412 |
GRECO ISOTHANE 1085A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength | 38.0 - 50.0 MPa | 5510 - 7250 psi | DIN 53455 |
Isoflon PVDF Polyvinyl Dichloride Fluoropolymer Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-100EL63 A1G Polymer Alloy, Elastomer Modified Main Characteristics: Rubbery; Soft; High shock absorption; High impact resistance; Elongation > 300%Applications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automitve Technol.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1495EC Polyester Based TPU Good extrusion stability, high transparency, excellent mechanical propertiesInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 38.0 MPa @Temperature 23.0 °C |
5510 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT™ 2062 Polyimide, Anthrazit Gleamy, 15% Graphite, 10% PTFE (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Tensile Strength | 38.0 - 42.0 MPa | 5510 - 6090 psi | ASTM D638 |
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor.. |
|||
Tensile Strength | 38.0 MPa | 5510 psi | after storage in water at 80°C for 42 days; ISO 37 |
BASF Elastollan C 88 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and chemical resistance, outstanding wear resistance, high tear and tensile strength, good damping c.. |
|||
Tensile Strength | 38.0 MPa @Strain 15.0 %, Temperature 60.0 °C |
5510 psi @Strain 15.0 %, Temperature 140 °F |
50 mm/min; ISO 527-2 |
BASF Elastollan R 1000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Tensile Strength | 38.0 MPa @Strain 300 % |
5510 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 64 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | >= 38.0 MPa | >= 5510 psi | ISO 37 |
Austin Novel Materials Texalan® 285A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Strength | >= 38.0 MPa | >= 5510 psi | ISO 37 |
Austin Novel Materials Texalan® 585A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Strength | >= 38.0 MPa | >= 5510 psi | ISO 37 |
Austin Novel Materials Texalan® 790A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tensile Strength | >= 38.0 MPa | >= 5510 psi | ISO 37 |
Austin Novel Materials Texalan® 482A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Strength | 38.0 MPa | 5510 psi | ASTM D412 |
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |