Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D638 |
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D638 |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D638 |
Premix Premi-Glas® 3101-20 Polyester BMC Premi-Glas® 3101-20 a 20% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL 94-.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D638 |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D638 |
Premix Premi-Glas® 3101-25 Polyester BMC Premi-Glas® 3101-25 is a 25% glass reinforced thermoset Bulk Molding Compound designed for electrical and flame retardant applications. Key features and benefits are: Underwriters Laboratories, UL .. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D638 |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D412 |
GRECO ISOTHANE 3080AF Polyether TPU Resin ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1101 A (SBS) Liner Block Copolymer Description: Kraton D1101 A polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1101 B (SBS) Liner Block Copolymer Description: Kraton D1101 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from South America in the physical form(s) identifi.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1101 E (SBS) Liner Block Copolymer Description: Kraton D1101 E polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ISO 37 |
Kraton® D1101 J (SBS) Liner Block Copolymer Description: Kraton D1101 J is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Japan in the physical form(s) outlined in the follow.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1102 B (SBS) Liner Block Copolymer Description: Kraton D1102 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 29.5%. It is supplied from South America in the physical form identifie.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1102 E (SBS) Liner Block Copolymer Description: Kraton D1102 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 28.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ISO 37 |
Kraton® D1155 B (SBS) Liner Block Copolymer Description: Kraton D1155 B is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from South America as indicated in the grade nomenclature.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | DIN 53455 |
Isoflon PP Polypropylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D412 |
GRECO ISOTHANE 1075A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D412 |
GRECO ISOTHANE 1080AF Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 FDA series products are poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance and solvent resistance. These products can be inject.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D412 |
GRECO ISOTHANE 2075A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | measured on films cast from a solution in toluene; ISO 37 |
Kraton® D1102 A (SBS) Liner Block Copolymer Description: Kraton D1102 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ISO 37 |
Kraton® D1102 J (SBS) Liner Block Copolymer Description: Kraton D1102 J is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Japan in the physical form(s) identified below in the.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D412 |
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Tensile Strength | 33.0 MPa @Strain 300 % |
4790 psi @Strain 300 % |
ISO 37 |
BASF Elastollan 1154 D FHF TPUR Flame Retardant Halogen Free Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | 50 mm/min; ISO 527-2 |
CENTROPLAST CENTROLAB HT Polypropylene Higher Temperatures PP-HT is a semi-crystalline plastic, with high acid and chemical resistance and mechanical strength. Due to its high resistance to temperature, PP-HT-plastics are often used in medical technology as.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ISO 527 |
Bulk Molding Compounds BMC 665 Mineral Filled, Glass Reinforced Polyester BMC 665 molding compound is a mineral filled, glass reinforced polyester molding compound suitable for compression, transfer or stuffer injection molding. It is characterized by good moldability, o.. |
|||
Tensile Strength | 33.0 MPa | 4790 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |