Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 32.4 MPa | 4700 psi | ASTM D638 |
Quadrant EPP Durapro® Truck Liners (ASTM Product Data Sheet) |
|||
Tensile Strength | 32.4 MPa | 4690 psi | ISO 527 |
Gromax 1163LL TPE 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext.. |
|||
Tensile Strength | 32.4 MPa | 4700 psi | ASTM D638 |
Techmer ES Luriblend® TPX-HDPE-99018 Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc. |
|||
Tensile Strength | 32.4 MPa | 4700 psi | ASTM D638 |
Ensinger Tecatron® XP-69 Compression Molded PPS Compound, 35% Fiberglass and Mineral Filled Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Strength | 32.4 MPa | 4700 psi | 2 in/min; ASTM D638 |
Braskem CP360H Homopolymer Polypropylene Description: Narrow MWD, Low Smoke / CondensateApplications: Suggested Uses Include Fine Denier Spunbond Nonwovens, High-Speed Spinning - Continuous Filament YarnThis resin meets the requirements fo.. |
|||
Tensile Strength | 32.4 MPa | 4700 psi | |
AlphaGary Garathane™ 9006 Polyurethane based compound A non-blooming, flame retarded, 90°C rated, polyether based polyurethane compound for demanding wire and cable applications. |
|||
Tensile Strength | 32.4 MPa | 4700 psi | 2 in/min; ASTM D638 |
Braskem CP1200B Homopolymer Polypropylene Description: General PurposeApplications: Suggested Uses Include CompoundingThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug A.. |
|||
Tensile Strength | 32.4 MPa | 4700 psi | |
AlphaGary Garathane™ 9005 Polyurethane based compound 90°C rated flame retardant, polyether based, polyurethane compound for demanding cable jacket applications |