Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 3.30 MPa | 478 psi | ASTM D412 |
Northstar Polymers MPA-A30B Mold-Making Resin MPA-A30B is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Tensile Strength | 3.30 MPa @Strain 300 % |
479 psi @Strain 300 % |
ISO 37 |
BASF Elastollan S 50 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 3.30 MPa | 479 psi | ISO 37 |
AlphaGary Evoprene™ 047 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
Tensile Strength | 3.30 MPa | 479 psi | average; perpendicular to plane; ASTM C297 |
3A Composites Core Materials AIREX® T92.130 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |
|||
Tensile Strength | 3.30 MPa | 479 psi | ISO 37 |
AlphaGary Evoprene™ GC 5654 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |
|||
Tensile Strength | 3.30 MPa @Strain 100 % |
479 psi @Strain 100 % |
ISO 37 |
BASF Elastollan S 70 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |