Polymer Property : Tensile Strength = 28.35 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 28.35 MPa

@Treatment Temp. 136 °C,
Time 605000 sec
4112 psi

@Treatment Temp. 277 °F,
Time 168 hour
Air Oven aged
S&E Specialty Polymers GA-1046CTLF PVC
Application: Lead free 105° C tri-rated semi-rigid insulation compound suitable for UL style 1061, CSA-SRPVC, MIL-I-16878.Information provided by S&E Specialty Polymers