Mechanical Properties Metric English Comments
Tensile Strength 21.0 MPa
3050 psi
50 mm/min - CH; ISO 527
Nyco NYLITE® Wollastonite in Polypropylene
Data for polypropylene reinforced with 15% Nyco NYLITE® Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3) is a natur..
Tensile Strength 21.0 MPa
3050 psi
Cured State
Palm Labs Adhesives TURBO FUSE SERIES 155-HT (700 cp HIGH TEMPERATURE) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190-HT advanced formula is designed to polymerize instantly by absorbing surface moisture and is recommended for..
Tensile Strength 21.0 MPa
3050 psi
Cured State
Palm Labs Adhesives TURBO FUSE SERIES 190-HT (4000 cp HIGH TEMPERATURE) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190-HT advanced formula is designed to polymerize instantly by absorbing surface moisture and is recommended for..
Tensile Strength 21.0 MPa
3050 psi
at Yield; ISO 527-1/-2
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data)
TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion..
Tensile Strength 21.0 MPa
3050 psi
at Yield; ISO 527-1/-2
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data)
TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance
Tensile Strength 21.0 MPa
3050 psi
Optimum; With provided formulation; ASTM D638
PolyOne Geon™ 120 Series 120X400 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 120X400 is medium molecular weight resin providing a good balance of fusion temperatures and film physical properties. It gives good chemical foamability for producing medium to high density ..
Tensile Strength 21.0 MPa
3050 psi
Optimum; FF; ASTM D638
PolyOne Geon™ 120 Series 121AR Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Pac..
Tensile Strength 21.0 MPa
3050 psi
Optimum; With provided formulation; ASTM D638
PolyOne Geon™ 130 Series 138 Polyvinyl Chloride Copolymer (PVC Copolymer)
Geon® 138 is a vinyl ester copolymer dispersion resin, exhibiting fast fusion at low processing temperatures, resulting in energy savings and the ability to work with heat sensitive substrates. The..
Tensile Strength >= 21.0 MPa
>= 3050 psi
ISO 37
Austin Novel Materials Texalan® 670A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech
Copyright © lookpolymers.com All Rights Reserved