Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 2.45 MPa | >= 356 psi | ASTM D 638 |
Karina 300-40/236 Green PVC Compound For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 2.45 MPa | >= 356 psi | ASTM D 638 |
Karina 35/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 2.45 MPa | >= 356 psi | ASTM D 638 |
Karina 350-02/249 Yellow PVC Compound For footware.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |