Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2.20 MPa | 319 psi | ISO 37 |
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Tensile Strength | >= 2.20 MPa | >= 319 psi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Tensile Strength | >= 2.20 MPa | >= 319 psi | in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Tensile Strength | 2.20 MPa | 319 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to .. |
|||
Tensile Strength | 2.20 MPa | 319 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Tensile Strength | 2.20 MPa | 319 psi | average; in the plane; ISO 527 1-2 |
3A Composites Core Materials AIREX® C71.75 Elevated Temperature Structural Foam AIREX® C71 is a closed cell, crosslinked polymer foam especially formulated to maintain its stability also at higher processing or service temperatures. It combines excellent stiffness and strength.. |
|||
Tensile Strength | 2.20 MPa | 319 psi | ISO 37 |
AlphaGary Evoprene™ GC 5685 SEBS Thermoplastic Elastomer Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can.. |