Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 186.39 MPa | 27034 psi | ASTM D638 |
E-Polymers SEPAZ® V230A 30% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |