Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 1610 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 1610 MPa
234000 psi
48 HRC
Schmolz + Bickenbach Thermodur® 2367 Superclean Hot Work Die Steel
Description: Thermodur® 2367 Superclean is an electro slag remelted (ESR) hot work die steel developed for applications where high temperature properties (tensile strength & thermal conductivity)..
Copyright © lookpolymers.com All Rights Reserved