Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 15.55 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 15.55 MPa

@Treatment Temp. 60.0 °C,
Time 605000 sec
2255 psi

@Treatment Temp. 140 °F,
Time 168 hour
Oil oven aged
S&E Specialty Polymers GA-1941-AFRO PVC
Application: 105° C PVC insulating compound designed for SJEOO applicationsInformation provided by S&E Specialty Polymers