Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina E 911D40/77-IS Green PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | NBR NM-IEC 60811-1-1 |
Karina E MCP 520 Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 80/213-D-IS-SI Clear PVC Compound (DAY Brazil) Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 800-10/10-IS White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 800-25/1-IS Natural PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 800D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection and extrusion of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 813D02/28-IS Yellow PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 813D11/4-IS-AS Bronze PVC Compound Heavy metal free and UV resistant compound, recommended for extrusion of refrigeration chamber curtain.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 813D40/88-IS-AS Green PVC Compound Heavy metal free and UV resistant compound, recommended for extrusion of refrigeration chamber curtain.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | NBR NM-IEC 60811-1-1 |
Karina 813D43/46-IS-AS Red PVC Compound Heavy metal free and UV resistant compound, recommended for extrusion of refrigeration chamber curtain.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 85/227-D-AT-IS-SI Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 85/277-D-AT-IS Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | NBR NM-IEC 60811-1-1 |
Karina 851D48/1-A-IS-LMP Black PVC Compound Heavy metal free PVC compound class 70C (ST1), recommended for electrical flexible cables jacketing. Also suitable for injection of plug.Information provided by Karina Indústria e Comércio de.. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 900-35/1-AYR-AC-LF Ivory PVC Compound Flame retardant and heavy metal free PVC compound, recommended for insulation of automotive electrical cables for working at the temperature range of -40°C to 105°C.Information provided by Kar.. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 900D06/469-AT-IS Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina 95/222-D-AT-IS Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | NBR NM-IEC 60811-1-1 |
Karina E 75800-35/1-B-AC Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina E 80/200-D-IS Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina E 85/227-D-AT-IS-SI PVC Compound Clear PVC compound recommended for cling films.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina E 85/243-DA-AT-IS-SI Clear PVC Compound Clear PVC compound recommended for cling films; Food grade, North AmericaInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina E 85/269-K-AT-IS-SI Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina E 87/206-D-AT-IS-SI Clear PVC Compound Crystal flexible PVC compound, recommended for extrusion of stretch films for general packaging.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina E 880-10/136-A-IS-As White PVC Compound Anti-UV and anti-fungus additivated PVC compound, recommended for general extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 14.7 MPa | >= 2130 psi | ASTM D 638 |
Karina E 890-25/1-CR-IS Natural PVC Compound Flame retardant and oil resistant PVC compound, recommended for thin wall insulation of automotive electrical wires for working at the temperature range of -40°C to 105°C.Information provided .. |
|||
Tensile Strength | 14.7 MPa | 2130 psi | |
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Tensile Strength | 14.7 MPa | 2130 psi | |
Taiwan Sheen Soon Sheenthane® A8510 TPU for Ink Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati.. |
|||
Tensile Strength | 14.7 MPa | 2130 psi | |
Taiwan Sheen Soon Sheenthane® A9070A Film Grade Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD. |