Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 132 MPa | 19100 psi | ASTM D638 |
Kolon SPESIN® KP212G30V0NB G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, high flowApplications: A variety of cases and connectorsInformation provided by API-Kolon. Information provided by API-Kolon. |
|||
Tensile Strength | 132 MPa | 19200 psi | ASTM D638 |
Gromax PBT 4140-201D 40% Glass Fiber Filled Product Description: A glass fiber 40% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Tensile Strength | 132 MPa | 19200 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BFG30-EN03N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 132 MPa | 19200 psi | 50 mm/min; ISO 527 |
Gromax BTG30-FN03N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 132 MPa | 19200 psi | ASTM D638 |
Samyang Tramid® 210G15 Polyamide, Reinforced Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210G15 is a reinforced grade.Applications:Automotive gear level housingConnectors.. |
|||
Tensile Strength | 132 MPa | 19200 psi | ASTM D638 |
Gromax CCP PBT 3040-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |