Mechanical Properties Metric English Comments
Tensile Strength 13.05 MPa
1893 psi
Average; ASTM D412 Method A
Seals Eastern 7042 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..