Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 127 MPa | 18500 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 127 MPa | 18500 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® T102G30 PET, 30% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 127 MPa | 18500 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 127 MPa | 18500 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 127 MPa | 18500 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 127 MPa | 18500 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 127 MPa | 18500 psi | ASTM D638 |
Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Tensile Strength | 127 MPa | 18300 psi | ASTM D638 |
Gromax CCP PBT 3030-200HR 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |