Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 124 MPa | 18000 psi | |
Poco Graphite SUPERSiC® Si Silicon Carbide The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for.. |
|||
Tensile Strength | 124 MPa | 18000 psi | ASTM D638 |
Quadrant EPP Duratron® PAI T4503 Compression Molded, Polyamide-imide, Eelectrical Grade (ASTM Product Data Sheet) |
|||
Tensile Strength | >= 124 MPa | >= 18000 psi | |
H.C. Starck Grain Stabilized Niobium (GSNb) GSNb is a patent pending single-phase micro-alloy that has a grain size of approximately 2 ASTM numbers finer than standard commercial grade niobium.Applications: Grain Stabilized Niobium (GSNb) is.. |
|||
Tensile Strength | 124 MPa | 18000 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-120NA and R-7-120BL glass fiber and mineral filled polyphenylene sulfide compounds provide good strength and low maintenance molding using conventional molding equipment.Features: Good.. |
|||
Tensile Strength | 124 MPa | 18000 psi | ASTM D638 |
Solvay Specialty Polymers Ryton® XE4050BL Polyphenylene Sulfide Alloy (PPS Alloy), GlassMineral Filled Ryton® XE4050BL glass fiber and mineral filled polyphenylene sulfide alloy compound provides high ductility and impact strength along with good thermal stability.Features: Ductile; Good Thermal S.. |
|||
Tensile Strength | 124 MPa | 18000 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |
|||
Tensile Strength | 124 MPa @Temperature 23.0 °C |
18000 psi @Temperature 73.4 °F |
EN ISO 527 |
Ensinger TECASINT 4011 Polyimide, Yellow (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Tensile Strength | 124 MPa | 18000 psi | ASTM D638 |
E-Polymers SEPAZ® V220A 20% Glass Fiber Reinforced PPA Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s.. |
|||
Tensile Strength | 124 MPa | 18000 psi | |
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Tensile Strength | 124 MPa | 18000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Flame RetardantFeatures: Flame Retardant UL File Number: E157318Processing Met.. |