Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 108 MPa | 15700 psi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU)
(Unverified Data**) Udel GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Tensile Strength | 108 MPa | 15700 psi | ASTM D638 |
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin G/F 20% reinforced, weather resistanceApplications: Parts of electric lightInformation provided by API-Kolon. |
|||
Tensile Strength | 108 MPa | 15700 psi | ASTM D638 |
Kolon SPESIN® KP213G30SB3 Glass Fiber Reinforced PBT Compound Resin G/F 30% reinforcedApplications: Ignition coil bobbinsInformation provided by API-Kolon. |
|||
Tensile Strength | 108 MPa | 15600 psi | ASTM D638 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Tensile Strength | 108 MPa | 15600 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BFG15-DN00N1 Nylon 6 16% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 108 MPa | 15700 psi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber Udel® GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Tensile Strength | 108 MPa | 15600 psi | ASTM D638 |
Samyang Tribit® 1500G20 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G20 is a reinforced, general purpose gr.. |
|||
Tensile Strength | 108 MPa | 15700 psi | ASTM D638 |
Aaron Industries AAROPRENE® GFPC 5020 Glass Filled Polycarbonate AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |