Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 10.3 MPa | >= 1490 psi | ASTM D412 |
S&E Specialty Polymers G-04-036ESD PVC Application: High Performance, PVC based compound with antistatic properties. G-04-036ESD is suitable for Gamma radiation sterilization.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D638 |
Quadrant EPP Fluorosint® 207 PTFE, Compression Molded Synthetic Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B90T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 10.3 MPa @Strain 100 % |
1490 psi @Strain 100 % |
Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV-3766 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 2900 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation .. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 2940 Compressed Aramid Fiber Gasketing, SBR Binder Aramid fibers with a Styrene-Butadiene (SBR) Binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasol.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 2950 Compressed Aramid Fiber Gasketing, Nitrile Binder Aramid fibers with a nitrile binder.Ideal for utility servicesExcellent sealabilityImproved thermal stabilityGood for general serviceMedia: Water, aliphatic hydrocarbons, oils, gasolineInformation .. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 362 Nitrile Sheet Rubber Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #362 is a white nitrile sheet made from FDA-approved ingredients per Z1 CFR 177.2600. I.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 509 Butyl Sheet Rubber Style #509 is a branded, chloro-butyl sheet rubber product.Information provided by Garlock Rubber Technologies |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 5260 Neoprene Sheet Rubber This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 5360 Nitrile Sheet Rubber Nitrile sheet is primarily used for applications where resistance to oil, solvents and fuels is required.Style #5360 is a medium-hard, premium-grade nitrile sheet, also available in 40, 50, 70 and 8.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 5500 Compressed Inorganic Fiber Gasketing, Nitrile Binder Inorganic fibers with a nitrile binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal sea.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | across grain; ASTM F152 |
Garlock 5507 Compressed Inorganic Fiber Gasketing, EPDM Binder Inorganic fibers with an EPDM binder.Inorganic fiber gasketing offers excellent thermal stability with minimal weight lossReduced creep relaxation and improved torque retention provide optimal seala.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | |
Garlock 7797 Neoprene Sheet Rubber This blended neoprene sheet is used where good oil, petroleum, ozone and weathering-resistance is needed.Black, smooth cloth finishInformation provided by Garlock Rubber Technologies |
|||
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D412 |
Garlock 7992 Neoprene Rubber Diaphragm, Fabric Insert Neoprene rubber with 22oz. hose duck fabric insertCombines elasticity and extensibility of rubber with strength of fabric insert. Specially compounded in varying burst strengths for almost any serv.. |
|||
Tensile Strength | 10.3 MPa | 1490 psi | ASTM D412 |
Kraton® G1643 M (SEBS) Linear Triblock Copolymer Description: Kraton G1643 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 20%. It is supplied from North America in the physical form ide.. |
|||
Tensile Strength | 10.3 MPa | 1490 psi | |
Momentive Performance Materials TSE 2267 Heat Cured Rubber - High Duro Translucent Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tensile Strength | >= 10.3 MPa | >= 1500 psi | ASTM D412 Method A |
Seals Eastern 7040 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Strength | 10.3 MPa | 1490 psi | ASTM D638 |
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Silicone Property; ASTM D412 |
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported) Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Silicone Property; ASTM D412 |
Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary Garathane™ X 05-309 A3 Polyurethane based compound Abrasion & Slip Resistant |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC 2215/3X-55 Black 1000 Polyvinyl Chloride Thermoplastic Molding grade for grommets and connectors with fungus resistance |
|||
Tensile Strength | 10.3 MPa | 1500 psi | Adhesion |
Atom Adhesives AA-DUCT 905 Epoxy Adhesive AA-DUCT 905 is a single component epoxy, formulated with pure silver powder combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti.. |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC 7731 Polyvinyl Chloride Thermoplastic Automotive Molding |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC GM 5055 Natural Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC GM 5065 Natural Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Tensile Strength | 10.3 MPa | 1500 psi | |
AlphaGary PVC GM 5075 Polyvinyl Chloride Thermoplastic A 105°C rated, lead & cadmium free, UL-94 V2 molding compound |
|||
Tensile Strength | 10.3 MPa | 1500 psi | ASTM D638 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |