Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 1.03 MPa | 149 psi | Typical; ASTM D3574-75 Test E |
Rogers Corporation Poron® 4701-41-30 Urethane Foam, Soft, Enhanced Sealability Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements. Standard available thickness range from 0.031".. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® 6503 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® 6510 Conductive Elastomer Extruded onlyInformation provided by Chomerics |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics Tecknit NC-Consil® FR750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics ParPHorm® 1800 Non-Conductive Form-in-Place Gasket Description: A range of conductive particle technologies combined with thermoset and RTV silicone systems provide a material selection for most opportunities. Multiple filler grades balance material.. |
|||
Tensile Strength | 1.03 MPa | 150 psi | Die A; ASTM D412 |
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK5151 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ P391SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ P392SHD EPDM Note 1: The Durafoamâ„¢100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from .. |
|||
Tensile Strength | >= 1.03 MPa | >= 150 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® 6502 Conductive Elastomer Description: Highest performance in harsh environments; excellent shielding; best choice for corrosion requirements against aluminum.Molded and ExtrudedRoHS CompliantInformation provided by Chomeric.. |