Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 0.500 MPa | 72.5 psi | ASTM D 412 |
Eurofoam Porocell POR 301/F NR-SBR Foam Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.500 MPa | 72.5 psi | ASTM D 412 |
Eurofoam Porocell POR 300/60 Ethylene Octane Metallocene EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.500 MPa | 72.5 psi | ASTM D 412 |
Eurofoam Porocell POR 304 CM-KPA 45 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tensile Strength | 0.500 MPa | 72.5 psi | |
BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe) Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th.. |