Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 1.00 N | 0.225 lb (f) | TD; ISO 6383/2 |
Borealis Borstar® FB1460 HDPE for Film Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz.. |