Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 2.00 - 4.00 N | 0.450 - 0.899 lb (f) | Average value: 3.00 N Grade Count:7 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |