Polymer Property : Tear Strength, Total = 688.2 N Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength, Total 688.2 N
154.7 lb (f)
Die C; ASTM D1004
Teknor Apex Flexalloy® 3500-55 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MWUses- Tubing, Pump PartsForms-PelletsProcessing- ExtrusionInformation provided by Te..