Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 3.00 N | 0.674 lb (f) | MD; ISO 6383/2 |
Borealis Himod™ FT5270 LDPE for Film Himod FT5270 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Tear Strength, Total | 3.00 N | 0.674 lb (f) | Initial in TD; ASTM D1004 |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |