Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 29.4 J/cm | 55.0 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 106 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |