Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 160 J/cm | 300 ft-lb/in | ASTM D1822 |
Styron CALIBREâ„¢ 893-10 Polycarbonate CALIBREâ„¢ 893-10 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 1507 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 2532 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 3731 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 3780 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 4527 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 4527 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 4533 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 4533 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 4579 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 4579 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 477 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 6580 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Filling |
Hexcel® HexForce™ 5351 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 7580 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Filling Breaking Strength |
Hexcel® HexForce™ 341 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Tensile Impact | 160 J/cm | 300 ft-lb/in | Warp Breaking Strength |
Hexcel® HexForce™ 7532 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |