Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact | 130 J/cm | 244 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene LDPE 2404TC47 Light duty FilmIt is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.Information provi.. |
|||
Tensile Impact | 130 J/cm | 244 ft-lb/in | ASTM D4272 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Tensile Impact | 130 - 350 J/cm | 244 - 656 ft-lb/in | Average value: 225 J/cm Grade Count:13 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |